Calibrate Using the Keypad
| Use these instructions for keypad installations only. If a computer will be attached to the module, skip this section. All setup functions will be done in the analysis software application. |
The pycnometer volume should be calibrated every time it is restarted. Cell volume and expansion volume in the set up parameters are updated automatically upon calibration. Run an analysis with an empty cup to see how close the average volume is to 0. It should be ±0.05% of full scale. If it is not within ±0.05% of full scale, calibration is required.
If calibrating using the software, see Calibrate using the Software